There were some errors in the first column of Table 1. The correct table is given below:
SO1 | SO2 | SO3 | SO4 | SO5 | ||
---|---|---|---|---|---|---|
a Irradiation energy until 20% SO degradation. | ||||||
Mw | 328.41 | 404.50 | 495.61 | 523.67 | 378.47 | |
Stability of glass state | 1 day | 2,3 days | 2 months | 2 months | 2,3 days | |
Tg/K | 308 | 335 | 346 | 359 | 337 | |
λmax/nm | 612 | 622 | 635 | 641 | 598 | |
τ1/2/s | 3.7 × 101 | 3.5 × 103 | 9.6 × 102 | 2.9 × 103 | 3.7 × 103 | |
Photodurabilitya/J cm−2 | Air | 5.0 × 100 | 4.7 × 101 | 8.3 × 101 | 6.5 × 101 | 3.7 × 101 |
N2 | 1.6 × 102 | 6.7 × 102 | 6.9 × 102 | 3.7 × 102 | 9.2 × 102 |